==押出注意事項== *參考Hytrel Extrusion Manual *押出前需乾燥,使其含水率低於0.08% (P3 Dyer) *L/D=24 以上(P3 Extruder barrel) *壓縮比 2.5~3.5(P3 Screw design)[[螺桿LD比、壓縮比]] *單螺桿(P3 Materials of construction) **約等長的三段設計(供料.壓縮.計量) **For most Hytrel® extrusion purposes good results are obtained with simple 3-zone screws, having approximately equal length feed, transition (compression) and metering sections. The length-to-diameter (L/D) ratio should be ideally 24:1 or higher for good uniformity of extrudate (i.e., minimum temperature and pressure variations). Compression ratios should be between 2.5 and 3.5:1, as determined by the depth of feed zone channel divided by the depth of metering zone channel (“apparent compression ratio”) for constant pitch screws. The depth of channel in both feed and metering sections is important: if the feed channel is too deep and not sufficiently long, particularly with large diameter screws, it can cause poor feeding and irregular output with some harder Hytrel® types. https://dl.dropboxusercontent.com/s/1vfk1d5002yd8t7/PDFXEdit_2016-08-19_09-49-46.png *網目(#80以上 x2 P4 Screens and breaker plate) *押出溫度 https://dl.dropboxusercontent.com/s/ythlstebfhir69k/PDFXEdit_2016-08-19_10-02-42.png *抽真空外模尺寸選擇 https://dl.dropboxusercontent.com/s/9apxgx2vhq6apu7/PDFXEdit_2016-08-19_10-05-27.png
返回到「
Hytrel
」。
導覽選單
個人工具
建立帳號
登入
命名空間
頁面
討論
臺灣正體
視圖
閱讀
檢視原始碼
檢視歷史
更多
搜尋
導覽
首頁
近期變更
隨機頁面
MediaWiki說明
工具
連結至此的頁面
相關變更
特殊頁面
頁面資訊